摘要: 介绍了运用快燃物提高固体推进剂燃速的方法。在6.86MPa下,当添加快燃物ACP的量为5%时,丁羟推进剂燃速由73mm/s提高到119mm/s;且快燃物ACP对推进剂的安全性能没有明显不良影响。
关键词: 端羟基聚丁二烯推进剂;高燃速推进剂;燃速调节剂;燃烧性能
Abstract: A method of increasing the burning rate of solid propellants by adding fast burning energetic materials is introducedThe burning rate of HTPB propellants is greatly increased from 73mm/s to 119mm/s(686MPa) by adding 5 weight percent of fast burning energetic complex ACPACP has no poor effect on the safety properties of propellants